Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 60.0 kN/m | 342 pli | ISO 34 |
Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | Injection molded parts; DIN 53515 |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | |
Huntsman IROGRAN® A 85 P 4944 Ether-Based TPU-For Cable Industry High temperature stabilityInformation provided by Huntsman |
|||
Tear Strength | 60.0 kN/m | 342 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 60.0 kN/m | 342 pli | |
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact Extrusion grade; High microbial resistance, matte surfaceInformation provided by Huntsman |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN 53515 |
Lubrizol ESTANE® T4057 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 60.0 kN/m | 342 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN 53515 |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN 53515 |
Lubrizol ESTANE® 58888 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 60.0 kN/m | 342 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN 53515 |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN 53515 |
Lubrizol ESTANE® 58562 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 60.0 kN/m | 342 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR7018 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1085 A TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1185 A M TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan SP 806 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | |
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1185 A FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan 880 AN TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 75 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | |
AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tear Strength | >= 60.0 kN/m | >= 342 pli | ISO 34 |
Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 60.0 kN/m | 342 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 70 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 60.0 kN/m | 342 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |