Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Zinc Stearate

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.25 PHR Zinc Stearate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.Zinc stearate has replaced cadmium stearate due to toxicity concerns with cadmium compounds. Used as a coactivator with Thanecure® ZM it shortens cure times and improves compression set. Zinc stearate also functions as a process aid and release agent, and helps prevent sticking to mill or internal mixer surfaces.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 33.87 MPa
4912 psi
Elongation at Yield 559 %
559 %
100% Modulus 0.00423 GPa
0.614 ksi
200% Modulus 0.009735 GPa
1.412 ksi
300% Modulus 0.01668 GPa
2.419 ksi
Tear Strength 60.0 kN/m
342 pli
Die C
Compression Set 34.6 %

@Temperature 70.0 °C,
Time 79200 sec
34.6 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 8.40 min

@Temperature 155 °C
0.140 hour

@Temperature 311 °F
TC90
Users viewing this material also viewed the following: