Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applications: Shoe-soles, top pieces, tubes, technical parts e.g. castor tyres.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
ISO 868
Tensile Strength 50.0 MPa
7250 psi
ISO 37
2.00 MPa

@Strain 20.0 %
290 psi

@Strain 20.0 %
ISO 37
4.00 MPa

@Strain 100 %
580 psi

@Strain 100 %
ISO 37
8.00 MPa

@Strain 300 %
1160 psi

@Strain 300 %
ISO 37
Elongation at Break 750 %
750 %
ISO 37
Charpy Impact, Notched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
DIN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 60.0 kN/m
342 pli
DIN ISO 34-1/Bb
Abrasion 40
40
[mm<sup>3</sup>; ISO 4649
Compression Set 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ISO 815
35 %

@Temperature 70.0 °C
35 %

@Temperature 158 °F
ISO 815
Processing Properties Metric English Comments
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
175 - 240 °C
347 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding and Extrusion