Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.30 GPa | 914 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 25 Polyamide 6, 25% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 25% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | |
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ASTM D790 |
Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade
(discontinued **)&l Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which .. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
Grupo Repol Dinalon® B1S25 G30XV0 30% Glass Reinforced, V-0 Rated Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFP36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Silicone. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East) LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF006 ABS (Europe-Africa-Middle East) LNP* Thermocomp* AF006 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS (Europe-Africa-Middle East) LNP* Thermocomp* AF006XXZ is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF004 Is a compound based on Polyetheretherketone containg Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
Unitika A3130 PA6, 35% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ASTM D790 |
Tipco Tipcolene® SEB 300 - 30% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 30% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178-93 |
Wellman Wellamid® GF20-60 XE-BKDX9 Nylon 6, 20% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178-93 |
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6 Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ASTM-D790 |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ASTM D790, ISO 178 |
EPICHEM Epiter PBT GF 20 Polybutylene Terephthalate, 20% Glass Characteristics: 20% glass fibre filled |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ASTM D790 |
E-Polymers TEKAMID® TB120SG30 Impact Modified, 30% Glass Fiber Reinforced PA6, DAM 30% Glass Fiber reinforced, High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | cond; ISO 178 |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
BASF Petra® 7010 BK 5830 15% Glass Filled PET Description: Petra 7010 BK5830 is a 15% glass fiber reinforced, pigmented black injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | ISO 178 |
BASF Ultramid® B3WG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Flexural Modulus | 6.30 GPa | 914 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible |