Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.39 GPa | 782 ksi | DIN 53452; ASTM D790 |
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Flexural Modulus | 5.39 GPa @Thickness 3.20 mm |
782 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON PS4200 ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch.. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Kotec Carbotex KG-20F10 Polycarbonate, Wear Resistant, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p.. |
|||
Flexural Modulus | 5.39 GPa @Thickness 3.20 mm |
782 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Gromax PBT 4115-104D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 5.39 GPa @Thickness 3.20 mm |
782 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D 790 |
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Engine Cover SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Samyang Tribit® 1500G30K PBT, Reinforced Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G30K is a reinforced, impact grade.Appl.. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (.. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Samyang Tribit® 1551GN15 PBT, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN15 is a reinforced, flame retardant g.. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 5.39 GPa | 782 ksi | ASTM D790 |
PlastxWorld CEVIAN® B5523 15% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 5.39 GPa @Thickness 3.20 mm |
782 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |