Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I.. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Techmer ES HiFill® ABS GF10 LE 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by .. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene 27% Glass Reinforced Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |