Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.10 GPa | 450 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and impact performance |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
Nilit FRIANYL A63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AT-10GB/15KV Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledAramid Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (DAM)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Global PEI-110 Easy Flow, Polyetherimide Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-3250 42% Chalk-Filled Polypropylene Homopolymer INNOPOL® CS 1-3250 is a 42% chalk-filled polypropylene homopolymer compound /PP-H KD42 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-3250 is developed f.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | Conditioned; ISO 178 |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 15 mm/min; ASTM D790 |
LG Chemical 25SPE GPPS Heat resistance, Chemical resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Superior extrusion pr.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF13 L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES Luriblend® PP GF20 CC GL2 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: Chemically Coupled and LubricatedAppearance: BlackInf.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
Styron VELVEXâ„¢ 5250 SC Reinforced Elastomer/PP compound Overview: VELVEXâ„¢ 5250 SC Natural is a reinforced elastomer/PP compound which provides a unique property balance of good stiffness, impact and high heat resistance in combination with a nice so.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100L (DAM) Nylon 66, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
Ineos Nova 202W Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulationProperties were determined on injection molded specimens at 23° and 50% RH unless otherwise specified.Information provi.. |