Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.310 GPa | 45.0 ksi | at 1%; ASTM D790 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790M |
DSM Somos® 8110 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
Multibase Multi-Flex® A 8832 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Noise Damping Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation provided by Mult.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin Key Features: fractional melt flow, medium low modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convolu.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | 1% secant - transverse direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | transverse direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® C100 Polyethylene; Enhanced Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typi.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | Compression molded parts prepared according to ASTM D 1928, method 1, procedure B.; ASTM D790 |
Dow FINGERPRINT™ DFDA-7510 NT Linear Low Density Polyethylene Resin FINGERPRINT™ DFDA-7510 NT resin is produced using UNIPOL™ process technology. It is intended for use in micro irrigation tube, durable hose and tube, profile extrusion, and injection molded fitti.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | |
BASF Ultramid® 8270 HS PA6 (Dry) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Modulus | 0.310 - 0.483 GPa | 45.0 - 70.0 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Flexural Modulus | 0.310 GPa | 45.0 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |