LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ ETA-5061 Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: fractional melt flow, medium low modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convoluted tubingDescription: Hifax ETA-5061 fractional melt flow, blow molding grade thermoplastic olefin resin has good flexibility, processability and impact resistance. It was designed for various automotive under-the-hood apploications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
Tool, Montell
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Modulus 0.310 GPa
45.0 ksi
Tangent at 0.05 in/min; ASTM D790A
Impact Test 19.0 J

@Temperature -30.0 °C
14.0 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Tear Strength 110 kN/m
628 pli
ASTM D624