Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D4107 CU BLK Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.950 g/cc
0.930 - 0.950 g/cc
ASTM D792
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
ASTM D1238
Ash 4.0 - 10 %
4.0 - 10 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 42 - 48
42 - 48
ASTM D2240
Tensile Strength, Yield >= 6.89 MPa
>= 1000 psi
ASTM D638
Flexural Modulus 0.310 - 0.483 GPa
45.0 - 70.0 ksi
ASTM D790