Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Multibase Multi-Pro® 4615 X White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Techmer ES Luriblend® TPX-POM-01060 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Total PSC 536 Polystyrene Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Total PSC 585 Polystyrene Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D-790 |
Axiall CL-6380, CL-6380J Rigid PVC, Molding Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where vis.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-1734 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound BRC R409006/HR is a Type 1 / Grade 1 injection molding compound developed for hot runner applications. BRC R409006/HR meets the cell classification of 12454-B. BRC R409006/HR WHT has been designed.. |
|||
Flexural Modulus | 2.96 - 13.4 GPa | 430 - 1950 ksi | Average value: 8.50 GPa Grade Count:13 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 2.96 - 9.65 GPa | 430 - 1400 ksi | Average value: 7.58 GPa Grade Count:11 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D-790 |
Axiall 3101 Rigid PVC, Extrusion Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be.. |