Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 430 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.96 GPa
430 ksi
Tangent; ASTM D790
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.96 GPa
430 ksi
Tangent; ASTM D790
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Flexural Modulus 2.96 GPa
430 ksi
Tangent; ASTM D790
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black
Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Total 680 Polystyrene  (discontinued **)
Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend)
Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Techmer ES Luriblend® TPX-POM-01060
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 2.96 GPa
430 ksi
Tangent; ASTM D790
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Total PSC 529 Polystyrene
Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Total PSC 536 Polystyrene
Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Total PSC 585 Polystyrene
Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Ensinger Tecapeek® XP-117 Compression Molded PEEK Compound, 25% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-1734 20% Glass Fiber Reinforced, High Impact
Information provided by Asahi Thermofil
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Asahi Kasei Thermofil P-40TC-1156 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 2.96 GPa
430 ksi
ASTM D-790
Axiall 3101 Rigid PVC, Extrusion
Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be..
Flexural Modulus 2.96 GPa
430 ksi
Tangent; ASTM D790
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey
Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating