Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall CL-6380, CL-6380J Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall CL-6380, CL-6380J Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where visual monitoring of the process is needed. CL-6380J is UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.40 g/cc
1.34 - 1.40 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D-785
Tensile Strength, Yield 49.6 MPa
7200 psi
ASTM D-638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D-638
Flexural Strength 89.6 MPa
13000 psi
ASTM D-790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D-790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
0.700 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
0.534 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 128 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Oxygen Index 35 %
35 %
ASTM D-2863
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 12454
NSF std. 14/61, 50
Flow Ratio (Distance/Wall Thickness, 390-400°F) 150
Georgia Gulf Test
Users viewing this material also viewed the following: