Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.50 GPa | 363 ksi | 1.5mm/min; ISO 178:2001 |
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant) This supreme wear resistant grade contains a combined liquid/solid lubricant system, which allows for a coefficient of friction as low as 0.08. The material has outstanding Pressure-Velocity capabil.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Flexural Modulus | 2.50 GPa @Temperature 23.0 °C |
363 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANBLEND FS7 PC/ASA Blend with Improved Weather Resistance Information provided by Polykemi AB |
|||
Flexural Modulus | 2.50 GPa @Temperature 23.0 °C |
363 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANCOMP PP BN140 T5 Polypropylene Information provided by Polykemi AB |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Radici Radilon® S 38L Nylon 6 Radilon® S (homopolyamides) are normally used in cast and blown extrusion for the production of packaging films. Radilon® S grades can be extruded to a thickness varying from 20 mm to 100 mm.Appl.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex AS0039 ABS (Europe-Africa-Middle East) LNP* Faradex* AS0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This .. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU (Europe-Africa-Middle East) LNP* COLORCOMP* G1000-GY4A805-0 is a compound based on Polysulfone resin. Added features include: Custom Color Grey. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1105-8173 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Aardvark Polymers AARTEL® 800AM Rotational Molding Resin Aartel 800AM is a new antimicrobial grade that offers the same excellent physical and mechanical properties of standard Aartel grades plus the added benefit of protection against microbial growth, p.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
Mitsui APELâ„¢ APL6509T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Polyplastics Duranex® 2000 Polybutylene Terephthalate (PBT), High flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Polyplastics Tepcon M90 Acetal-copolymer (POM), General Information provided by PolyPlastics. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Polyram RamLloy PBB503 PC/ABS Alloy, Flame Retardant and Heat Stabilized Flame retardant and heat stabilized PC/ABS alloy for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D 790 |
Cossa Polimeri ESTABLEND 8500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ASTM D790 |
Ashley Polymers Ashlene® P254WO PPO A general purpose V-0 rated resin with high impact strength.Data provided by the manufacturer |
|||
Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |