Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | Tangent; ASTM D790 |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Techmer ES HiFill FR® ABS FR BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Techmer ES HiFill FR® ABS FR V2 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Spartech Sungard Ultra Weatherable Polycarbonate Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Spartech UltraTuf SG Polycarbonate Sheet Description: Polycarbonate SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8015 CL Availability: North AmericaForms: PelletsFeatures: CopolymerAppearance: Clear/TransparentInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.34 GPa @Thickness 3.17 mm |
340 ksi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
A. Schulman COMTUF® 506 Polycarbonate Information provided by A. Schulman. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
A. Schulman COMTUF® 506 Polycarbonate Information provided by A. Schulman. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Total PSI 825 Polystyrene Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such .. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Entec Hylex® P1017L1 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Clear/Transparent Information provided by Entec |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D-790 |
Axiall SP-7008 Rigid PVC, Molding Georgia Gulf SP-7008 is a rigid vinyl compound formulated for electrical fittings and molded parts requiring high impact strength and toughness.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
Asahi Kasei Thermofil P-20TC-1156 20% Talc Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
PolyOne Lubri-Tech™ 5209 S2 Natural A Acetal Copolymer, 9 Melt with Silicone
(discontinued **) Information provided by PolyOne™ Corporation |