Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSI 825 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Total Atofina
Trade Name PSI
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSI 825 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such as appliance housings, house wares, toys, and structural foam require this polymer to produce consistent parts. Advanced rubber particle size control makes 825 the choice for all high gloss applications.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Yield 50 %
50 %
ASTM D638
Tensile Modulus 2.28 GPa
330 ksi
ASTM D638
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Falling Dart Impact 14.11 J
10.41 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 91.1 °C
196 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 96.1 °C
205 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 88 %
88 %
60°; ASTM D523