Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.00 GPa @Temperature 23.0 °C |
290 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | |
Plastcom SLOVALEN PC 93 T 20 PP, 20% mineral filling, UV stabilization FeaturesModified PP for injection moulding with the content of 20 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ISO 178 |
Total Lacqrene® 4240(EU) High Impact Polystyrene
(discontinued **) LACQRENE® 4240 is a high heat resistance, high impact polystyrene for the extrusion industry. Good mechanical and thermal properties leads to the production of thermoformed articles of good rigidi.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 80-7014 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | DIN 53452; ASTM D790 |
Kolon Kopa® KN173HI Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
Lucent Polymers 66-41 Nylon 66, Toughened Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL008 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RL008 is a compound based on PA 66 containing PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | tangent; ASTM D790 |
Spartech EP5220 Calcium Carbonate Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX954 PPE+PA (Europe-Africa-Middle East) NORYL GTX954 is an unfilled grade with improved processability and optimised heat/impact balance. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
Total PS CPDS 822 Standard Flow, Non-Deca Polystyrene Total Petrochemicals Polystyrene 822 is a good flow, environmentally friendly high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good d.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM-D790 |
Polyram RamOfin PPC500 Polypropylene, Flame Retardant Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339T10L1 Talc Reinforced |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | ASTM Data |
BASF Capron® 8259 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8259 is a type 6 nylon injection molding graft copolymer developed for fastener applications requiring to abusive impact molding combined with a high level of pullout strength. It exhibits v.. |
|||
Flexural Modulus | 2.00 GPa | 290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East) NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r.. |