Mechanical Properties Metric English Comments
Flexural Modulus 1.98 GPa
287 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers UTTAP ES 10559 Polycarbonate Alloy
Polycarbonate Alloy – High temperature (HDT), high Impact, with excellent short and long term heat stability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative h..
Flexural Modulus 1.98 GPa
287 ksi
ASTM D790-1
Ineos Styrenics 473D High-Impact Polystyrene Resin (NAFTA)
Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa..
Flexural Modulus 1.98 GPa
287 ksi
Kuraray SEPTON® CM2 Compatibilizer
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
Flexural Modulus 1.98 GPa
287 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON SD000 PA12
LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.
Flexural Modulus 1.98 GPa
287 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS
LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic.
Flexural Modulus 1.98 GPa
287 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific)
LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A
Flexural Modulus 1.98 GPa
287 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp YF005
LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.98 GPa
287 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber.
Flexural Modulus 1.98 GPa
287 ksi
ISO 178
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin
Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj..
Flexural Modulus 1.98 GPa
287 ksi
ISO 178
DSM Fibre Intermediates Nyrim® 1525 (Glass), Conditioned
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Flexural Modulus 1.98 GPa
287 ksi
conditioned 15 days, 23°C - 50 % R.H.; ISO 178
Arkema Group Rilsan® Clear G170 Polyamide
Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use..
Flexural Modulus 1.98 GPa

@Thickness 3.20 mm
287 ksi

@Thickness 0.126 in
5.1mm/min; ASTM D790
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions...
Copyright © lookpolymers.com All Rights Reserved