Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.55 GPa | 225 ksi | |
Plastcom SLOVALEN PC 71 T 15 PP, 15% mineral filling FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches - pack.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | |
Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent; ASTM D790 |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent; ASTM D790 |
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Chord; 2 mm/min; ISO 178 |
Mytex Polymers AN16L-44 Polypropylene, Compounded Description: Compounded polypropylene produced for automotive exterior applications using Mytex® Technology.Key Applications: Body side moldingInformation provided by Mytex Polymers |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled Information provided by PolyPlastic Group. |
|||
Flexural Modulus | >= 1.55 GPa | >= 225 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ASTM D 790 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Entec Hypel® PEHD.8/.962 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
M. Holland Company PP200 Polypropylene Homopolymer High ESCRGood heat aging resistanceHomopolymerGood stiffnessApplications: AutomotiveHospital goodsHousehold goodsTable products |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade) ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1124NA Polypropylene Homopolymer CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN LOW SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATION |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp FFL21 PE LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp FFL21 PE (Asia Pacific) LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Spartech SP-1010 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2mm/min; ISO 178 |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 30% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade Total Petrochemicals Polypropylene 3862 is recommended for high speed melt spinning processes and multifilament yarns like bulk continuous filament (BCF) and continuous filament (CF) fibers. 3862 i.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Eastman Tritan MX710 Copolyester Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Eastman Tritan TX1000 Copolyester Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Carmel Olefins CAPILENE® R 50 Polypropylene Homopolymer CAPILENE® R 50 is a polypropylene homopolymer intended for injection molding, characterized by good flow properties combined with good balance of stiffness and impact. APPLICATIONS CAPILENE ® .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene Features:medium viscosityexcellent processabilitygood stiffnessenvironmental stress crack resistanceheat performanceminimal odor and tasteApplications:closuressmall applianceshousewarestoyscontains .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Multibase Multi-Flam™ 0103 HDPE NH Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingInformation provided by Multibase |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790A |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |