Material Notes:
LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0088 cm/cm

@Time 86400 sec
0.0088 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.0 MPa
4210 psi
ASTM D 638
Elongation at Break 4.2 %
4.2 %
ASTM D 638
Tensile Modulus 2.14 GPa
310 ksi
50 mm/min; ASTM D 638
Flexural Strength 27.0 MPa
3920 psi
ASTM D 790
Flexural Modulus 1.55 GPa
225 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.83 J/cm

@Temperature 23.0 °C
5.30 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C

@Thickness 3.20 mm
154 °F

@Thickness 0.126 in
unannealed; ASTM D 648