Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.700 GPa | 102 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Flexural Modulus | 0.702 GPa | 102 ksi | ASTM D790 |
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
Reliance Industries Relene E41003 Polyethylene Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff.. |
|||
Flexural Modulus | 0.700 - 8.60 GPa @Temperature -40.0 - 120 °C |
102 - 1250 ksi @Temperature -40.0 - 248 °F |
Average value: 2.76 GPa Grade Count:7 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 110-3561 LMDPE Rotational Molding Resin Description: ICORENE 110-3561 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Solvay TECHNYL® B 230 PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M3804 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium wa.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Borealis Borseal™ TD218BF Terpolymer for BOPP Film Borseal TD218BF is a C2/C4 terapolymer film resin.Borseal TD218BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film proc.. |
|||
Flexural Modulus | 0.705 GPa | 102 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 396 Ionomer DescriptionFormion® FI 3936is a 3% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, and impact. Formion F1 396U is UV stabilized to exceed .. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | Transverse Direct |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D 790 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Borealis Borseal™ TD210BF Terpolymer for BOPP Film Borseal TD210BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD210B.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Borealis Borseal™ TD211BF Terpolymer for BOPP Film Borseal TD211BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD211B.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | Transverse Direct |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, Conditioned Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Flexural Modulus | 0.703 GPa | 102 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Unitika EX-1222 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant
(disconti Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Flexural Modulus | 0.700 - 3.00 GPa | 102 - 435 ksi | Average value: 1.45 GPa Grade Count:42 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |