Polymer Property : Flexural Modulus = 13.1 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.210 - 13.1 GPa
30.5 - 1900 ksi
Average value: 2.42 GPa Grade Count:153
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Flexural Modulus 1.72 - 13.1 GPa
250 - 1900 ksi
Average value: 5.78 GPa Grade Count:42
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Flexural Modulus 12.4 - 13.1 GPa
1800 - 1900 ksi
ASTM D790
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Flexural Modulus 12.4 - 13.1 GPa
1800 - 1900 ksi
ASTM D790
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
ASTM D790
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound
The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 1403 Electrical Grade
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 1603 Multi-purpose grade
BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength
BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat..
Flexural Modulus 11.0 - 13.1 GPa
1600 - 1900 ksi
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant
BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound
BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers.
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound
BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext..
Flexural Modulus 9.65 - 13.1 GPa
1400 - 1900 ksi
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound
BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC A50-XHS Bulk molding compound
Description: BMC A50­XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in pre­weighted slugs. Due to the excellent flow and controlled reactivity, BMC A50­XHS i..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound
BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound
Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound
BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade
BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester
BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel..
Flexural Modulus 7.58 - 13.1 GPa
1100 - 1900 ksi
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound
BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings.
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 810 General Purpose Molding Compound
BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound
BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts...
Flexural Modulus 1.24 - 13.1 GPa
180 - 1900 ksi
Average value: 2.86 GPa Grade Count:96
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Modulus 2.10 - 13.1 GPa
305 - 1900 ksi
Average value: 4.73 GPa Grade Count:39
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound
BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi..