Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cubic inch savings. BMC T60-6002-WG-(15) can be injection, transfer and compression molded. It is UL listed and is typically used in power distribution equipment, switching components/relays, constant use switch applications and circuit protection breakers.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.62 - 1.82 g/cc
0.0585 - 0.0658 lb/in³
Molded
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
0.0015 - 0.0025 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 20 - 25
20 - 25
Tensile Strength 45.5 - 59.3 MPa
6600 - 8600 psi
Flexural Strength 170 - 193 MPa
24700 - 28000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 87.6 - 115 MPa
12700 - 16700 psi
Izod Impact, Notched 3.31 - 4.38 J/cm
6.20 - 8.20 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 14.2 - 16.2 kV/mm
361 - 411 kV/in
short time
Arc Resistance >= 188 sec
>= 188 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F