Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
NYCOA 5033 HS 33% Glass-Fiber Reinforced, Heat Stabilized, Nylon 66 Resin NYCOA 5033 HS is a 33% glass fiber reinforced, heat stabilized Nylon 66 resin used for injection molding. It offers an outstanding balance of mechanical properties over standard grades of convention.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2mm/min; ASTM D790 |
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GF006 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 (Asia Pacific) LNP* Thermocomp* QF007 is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EXZ PA 66 LNP THERMOCOMP* RF006EXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66 (Asia Pacific) LNP* Thermocomp* RF006LXP is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WX93111 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WX93111 is a compound based on Polybutylene Terephalate resin containing Flame retardant , Glass Fiber, Proprietary filler. Added features include : Improved CTI. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66 LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Plenco 6582 Phenolic, Briquette, Transfer Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized Characteristics: 30% glass fibre filled |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, Conditioned Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
BLUESTAR 203G30 PBT, 30% Glass Filled Typical Applications: Thinner wall partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Plenco 4311 Phenolic, Granular, Transfer Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excelle.. |
|||
Flexural Modulus | 8.90 GPa | 1290 ksi | ASTM D790 |
Resinoid 7201 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |