Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 L X MT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: SilverTPCI# 7210102Information provid.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 9864111Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Hydrolysis ResistantAppearance: BlackInformation provided by TP Composites, In.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and He.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF25 HS NAT 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 0685 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Chase Plastics CP Pryme® N140MGHSL (DAM) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
PolyOne Edgetek® ATH-25GF-10MN/000 Acetal-Homopolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedChemically CoupledInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
PolyOne Edgetek® ES-30GF/000 PES (Polyethersulfone), 30% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |