Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PBT GF30 HR BK 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Hydrolysis ResistantAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 141 MPa
20500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm
1.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 227 °C
440 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
407 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 20.5 kV/mm
520 kV/in
Method A (Short-Time); ASTM D149