Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.10 GPa | 885 ksi | Tangent; ASTM D790 |
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Radici Radilon® A RCV3015 RKC Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by GIT technology.Information provided by Radici group. |
|||
Flexural Modulus | 6.10 GPa @Temperature 23.0 °C |
885 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-G15 15% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific) LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, Conditioned Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black... |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KEL22A Acetal Homopolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL22A is a compound based on Acetal Homopolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN230GL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Plenco 7202 Phenolic, Granular, Injection Molded PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E4065.. |
|||
Flexural Modulus | 6.10 GPa @Temperature 160 °C |
885 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO Data |
BASF Ultradur B 4300 G4 BK5110 20% Glass Filled PBT Ultradur B 4300 G4 BK5110 is an easy flowing, pigmented black, injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Ashley Polymers Ashlene® 520-25GU Nylon 66, 25% Glass Reinforced Nylon 66, 25% glass reinforced resin, utility grade.Data provided by the manufacturer |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Excellent chemic.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178-93 |
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |