Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.10 GPa | 740 ksi | Tangent; ASTM D790 |
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL146 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL146 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | |
Plastcom SLOVALEN PH 69 GF 30 LS PP, 30% glass fibre, mod. of mech. prop., UV stability FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. UV stable. Increased strength in comparison with u.. |
|||
Flexural Modulus | 5.10 GPa @Temperature 90.0 °C |
740 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Nilit FRIANYL B63 HS-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.10 - 9.31 GPa | 740 - 1350 ksi | Average value: 7.66 GPa Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Global GPP-240C 40% Glass Reinforced, Chemically Coupled Impact Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 5.10 GPa @Thickness 3.20 mm |
740 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® SG3250 PBT+PET+MF25% Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | |
Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MFM43S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFM43S is a compound based on Polypropylene resin containing Glass Fiber, Mineral. Added features include : Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
PlastxWorld CEVIAN® B6524 20% GF PBT/ABS Alloy Glass fiber and mineral filled, low warpage and flame retarded PBT/ABS.Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Chase Plastics CP Pryme® N140MGHSL (COND, 50% RH) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178-93 |
Wellman Wellamid® GF13-66 XE-NBK1 13% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178-93 |
Wellman Wellamid® GFT1628-BK 17% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | 2mm/min; ISO 178 |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWUVCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO 178 |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO Data |
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-106 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | ISO Data |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Conditioned) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Flexural Modulus | 5.10 GPa | 740 ksi | STN EN ISO 178 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |