Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data provided by the manufacturer, Wellman Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Water Absorption 1.35 %
1.35 %
Approximate 24 hr.
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa
16000 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Flexural Yield Strength 175 MPa
25400 psi
ISO 178
Flexural Modulus 5.10 GPa
740 ksi
ISO 178
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.790 mm
HB

@Thickness 0.0311 in
Users viewing this material also viewed the following: