Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Shinil Chemical
Trade Name SHINSTRA
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technology with a variety of polymers to produce high performance SHINSTRA compound. SHINSTRA compounds are designed by alloying engineering thermoplastics or mineral reinforcing or fiber reinforcing or hybrid filler reinforcing. SHINSTRA are tailored to control the mechanical and physical properties according to its application or customer demand. SHINSTRA are often used to replace metal parts.Feature and BenefitsExcellent impact resistanceHigh scratch resistanceOutstanding abrasion resistanceExcellent chemical resistanceExcellent mechanical propertiesImproved thermal propertiesEasy processingLighter weightCost effectiveInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.7 MPa
12100 psi
Elongation at Break 4.0 %
4.0 %
Flexural Strength 113.8 MPa
16500 psi
Flexural Modulus 5.10 GPa
740 ksi
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F