Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Nylene® Naxel™ PC502 10% Glass Reinforced Polycarbonate Description: Naxel™ PC502 is a 10% glass fiber reinforced polycarbonate. PC502 is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companie.. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago |
|||
Flexural Modulus | 3.03 - 14.8 GPa | 440 - 2150 ksi | Average value: 7.75 GPa Grade Count:104 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PSU1700 Polysulfone General purpose polysulfone with excellent clarityAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | 2 mm/min; ISO 178 |
Lucite International Perspexâ„¢ XT Acrylic Extruded Sheet 0X00 PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES Electrablend® PC/ABS Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES Electrablend® PC/ABS 033009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® PA6 AF Colors Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid FiberAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricateAppearance: Colors AvailableInformation provi.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM CO 0150 S Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM CO 0167 S1 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM CO 0167 S2 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PKN4717 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Foam extrusion. Microwavable. Food packaging uses. Solid properties listed.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® PPSU A1 0200 B LE Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Total PSC 524B Polystyrene Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ensinger Tecapeek® XP-108 Compression Molded PEEK Compound, 20% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D-790 |
Axiall 6316 Rigid PVC, Molding Georgia Gulf 6316 is an economical high flow rigid PVC fittings compound designed for drain, waste and vent applications, where higher impact properties are desired. This compound is characterized .. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPS 100-1 GPPS BLACK Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A reprocessed, general-purpose Polystyrene resin, compounded black, specifically designed for all high speed injection molding appli.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | |
Abatron AboCast 8504-5 One-Component Epoxy AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D-790 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FM-2601 20% Glass/Mineral, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | secant; ASTM D790 |
Spartech PP5340 Mica Reinforced Homopolymer Information provided by Spartech |