Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Thermylene® P6-20FM-2601 20% Glass/Mineral, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P6-20FM-2601 20% Glass/Mineral, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 19 g/10 min
19 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Flexural Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.464 J/cm
0.870 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.9 °C
138 °F
ASTM D648
Users viewing this material also viewed the following: