Techmer ES HiFill® PPSU A1 0200 B LE

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PPSU A1 0200 B LE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 109 MPa
15800 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 18.9 kV/mm
480 kV/in
Method A (Short-Time); ASTM D149