Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Perspexâ„¢ XT Acrylic Extruded Sheet 0X00

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Extruded
Manufacturer Lucite International
Trade Name Perspex™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Lucite International Perspexâ„¢ XT Acrylic Extruded Sheet 0X00.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information provided by Lucite International.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 101
101
ISO 2039-2
Tensile Strength, Ultimate 70.0 MPa
10200 psi
5 mm/min; ISO 527
Elongation at Break 4.0 %
4.0 %
5 mm/min; ISO 527
Flexural Strength 107 MPa
15500 psi
2 mm/min; ISO 178
Flexural Modulus 3.03 GPa
439 ksi
2 mm/min; ISO 178
Charpy Impact Unnotched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 78.0 µm/m-°C

@Temperature 20.0 °C
43.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Vicat Softening Point >= 105 °C
>= 221 °F
ISO 306A
Flammability, UL94 HB
HB
Flammability Test 4.0
4.0
BS 476, Pt7
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489/A
Transmission, Visible >= 92 %
>= 92 %
clear grade; in 3 mm (colored grades lower); ASTM D1003