Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.5 GPa | 2250 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Flexural Modulus | 15.5 GPa @Temperature 23.0 °C |
2250 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | 25 mm/min; ISO 178 |
PolyOne Nymax™ GF 1200 A 55 HS Black 13 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | Conditioned; ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | |
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Kuraray Genestarâ„¢ GX1500A-M41 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. This grade was developed specifically for high mechanical properties for TD direction.Main Features:Low warpageHigh mechanical properties for TD directionExamp.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | 2 mm/min; ISO 178-A |
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00ASXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Solvay Technyl Starâ„¢ S 218 V50 50% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Polyplastics FR-PET® B3045FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ISO 178 |
Polyplastics Duranex® 702MS Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ASTM-D790 |
Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | Dry; ASTM D790 |
Asahi Kasei Leona® 90G50 50% Glass Filled Nylon 66 Enhanced strength and stiffness; with 50% GF. Excellent appearance.Applications:Office furnitureInformation provided by Asahi Kasei |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | DIN 53 457 |
Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only) Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Lamp Holders, Lamp SocketsProcessing: Inj.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 636 Nylon 6/6, Carbon Fiber Reinforced, Proprietary Lubricant Package Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ASTM-D790 |
Polyram Polytron A50N02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 15.5 GPa | 2250 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |