Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
Manufacturer Polyplastics Co.
Trade Name Duranex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Duranex® 702MS Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, GF filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives. Various grades are available, including flame-retardant, reinforced, and impact-resistant grades. DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts. DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 153 MPa
22200 psi
ISO 527-1, 2
Elongation at Break 1.3 %
1.3 %
ISO 527-1, 2
Flexural Strength 205 MPa
29700 psi
ISO 178
Flexural Modulus 15.5 GPa
2250 ksi
ISO 178
Charpy Impact, Notched 0.650 J/cm²
3.09 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 197 °C
387 °F
ISO 75-1, 2
Flammability, UL94 HB
HB