Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.42 GPa | 206 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 30-2000 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.42 - 17.9 GPa | 206 - 2600 ksi | Average value: 2.49 GPa Grade Count:112 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2mm/min; ASTM D790 |
3M Dyneon™ PVDF 1012/0180 Polyvinylidene Fluoride
(discontinued **) Improved clarity and flexibility compared to PVDF 1012/0001Improved impact strengthImproved processing compared to PVDF 1012/0001Improved drawabilityExcellent for filament sizes 6 to 30 milsInformat.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
PolyOne Edgetek® NJ-000/000 Nylon 12
(discontinued **) Description/Features:General Purpose GradeHeat StabilizedHigh FlowUL 94 HBProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
Hyosung Topilene J340E PP J340E Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
Hyosung Topilene J642 PP J642 Injection Impact CopolymerApplications:Washing M/C partsElectric applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
Hyosung Topilene S905H PP S905H Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.42 GPa @Thickness 6.40 mm |
206 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0952 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X6800BM PBT Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
Styron LGF 7600 Polypropylene Overview: STYRON LGF7600 is intended for use injection molding applications that require high stiffness. The material has good processability and fast cycle times. It contains nucleating agent. LGF .. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P700J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | |
Zylog Hipolyene® 8110 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – C.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East) Blow moldable, impact modifed XENOY |
|||
Flexural Modulus | 1.42 GPa | 206 ksi | ASTM D790 |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |