Improved clarity and flexibility compared to PVDF 1012/0001Improved impact strengthImproved processing compared to PVDF 1012/0001Improved drawabilityExcellent for filament sizes 6 to 30 milsInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Volatiles <= 0.20 %
<= 0.20 %
5 min/100°C, Thermobalance
Melt Index of Compound 6.5 g/10 min

@Load 10.0 kg,
Temperature 230 °C
6.5 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
50mm/min; ASTM D638
Tensile Strength, Yield 46.0 MPa
6670 psi
50mm/min; ASTM D638
Elongation at Break 95 %
95 %
ASTM D638
Elongation at Yield 12 %
12 %
50mm/min; ASTM D638
Flexural Modulus 1.42 GPa
206 ksi
2mm/min; ASTM D790
Descriptive Properties Value Comments
Color Opaque
Form Pellets