Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.700 GPa | 102 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Opnyl OP6MT254 Nylon 6 Nylon 6 – Mighty Tough plasticized extrusion grade for tubing/profile applications. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are p.. |
|||
Flexural Modulus | 0.700 GPa @Temperature 23.0 °C |
102 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Flexural Modulus | >= 0.700 GPa | >= 102 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant
(discont Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Flexural Modulus | 0.700 GPa @Temperature 90.0 °C |
102 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Flexural Modulus | >= 0.700 GPa | >= 102 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4436S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.700 GPa @Temperature 90.0 °C |
102 ksi @Temperature 194 °F |
ASTM D790 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
Reliance Industries Relene E41003 Polyethylene Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
Reliance Industries Relene L41003 Polyethylene The UV stabilized version of Relene E41003Information provided by Reliance Industries |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 110-3561 LMDPE Rotational Molding Resin Description: ICORENE 110-3561 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 115-3561 LMDPE Rotational Molding Resin Description: ICORENE 115-3561 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Solvay TECHNYL® B 238 Black 21 N PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium .. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM-D790 |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its spec.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Borealis Borseal™ TD210BF Terpolymer for BOPP Film Borseal TD210BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD210B.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
A. Schulman LP642 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 642 is a narrow molecular weight copolymer, high-density polyethylene combining high flow for thin wall articles with excellent toughness. ApplicationApplications of LP 642 include fo.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM D790 |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ASTM Test |
BASF Ultramid® 8255 HS PA6 (Dry) Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and
fle.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, Conditioned Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Unipetrol PE HD LITEN® VL 20 N HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | ISO 178 |
Unipetrol PE HD LITEN® VL 29 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.700 GPa | 102 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant
(disconti Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Flexural Modulus | 0.700 - 3.00 GPa | 102 - 435 ksi | Average value: 1.45 GPa Grade Count:42 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |