Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Total Atofina
Trade Name Lumicene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its specific molecular structure ensures: Superior mechanical propertiesOutstanding optical properties (gloss)Improved dimensional stabilityEasy processingInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133/D
135 g/10 min

@Load 21.6 kg,
Temperature 190 °C
135 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.0 MPa
1600 psi
ISO 527-2
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527-2
Elongation at Break >= 700 %
>= 700 %
ISO 527-2
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 123 °C
253 °F
ISO 11357
Vicat Softening Point 121 °C
250 °F
ISO 306