Mechanical Properties Metric English Comments
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)
Shear Strength 89.6 MPa
13000 psi
Notched Compression In-plane, Dry, RT; ASTM D3846-02
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III
Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures ..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
Shear Strength 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
Industrial Laminates/Norplex MC223 Cotton Fabric
Description: Grade MC223 is a medium weave cotton phenolic composite that is specifically formulated to meet MIL-P-18324.Typical applications include pintle and stave-type bearings for rudder shafts..
Shear Strength 89.6 MPa

@Thickness 15.7 mm
13000 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP315 Cotton Fabric
Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should ..
Shear Strength 89.6 MPa

@Thickness 15.7 mm
13000 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP319 Cotton Fabric Base Laminate
Description: Bleached canvas combined with phenolic resin and graphite lubricant. Better moisture resistance and machining characteristics than NP315.
Shear Strength 89.6 MPa

@Thickness 15.7 mm
13000 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
Shear Strength 89.6 MPa

@Thickness 15.7 mm
13000 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP639 Paper Base Laminate
Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T..
Shear Strength 89.6 MPa
13000 psi
Axial; ASTM D732
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Shear Strength 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
Industrial Laminates/Norplex MC330 Cotton Fabric
Description: Grade MC330 is a cotton cloth/phenolic resin composite which is specially processed to be used in cryogenic applications. Such applications include spacers for installation of liquid ox..
Shear Strength 89.6 MPa

@Thickness 15.7 mm
13000 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP310U Cotton Fabric
Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0...
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Shear Strength 89.6 MPa
13000 psi
Compression interlaminar; RT
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape
Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel
Shear Strength 89.6 MPa
13000 psi
Ultimate
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..
Shear Strength 89.6 MPa
13000 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)