Polymer Property : Tensile Strength, Ultimate = 6500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638-95
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene
This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase.
Tensile Strength, Ultimate 44.8 MPa
6500 psi
Mixed 1:1; TM R050-36
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Ultimate 44.8 MPa
6500 psi
TM R050-36
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
TM R050-36
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System
Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D412
PB1000-650 Polyurethane-based Biomedical Elastomer
Tensile Strength, Ultimate 44.8 - 110 MPa
6500 - 16000 psi
Average value: 74.2 MPa Grade Count:32
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Tensile Strength, Ultimate 44.8 - 121 MPa
6500 - 17500 psi
Average value: 69.7 MPa Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound  (discontinued **)
High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance..
Tensile Strength, Ultimate 44.8 - 131 MPa
6500 - 19000 psi
Average value: 55.4 MPa Grade Count:15
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
Tensile Strength, Ultimate 44.8 - 200 MPa
6500 - 29000 psi
Average value: 131 MPa Grade Count:141
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM Data
Styron Pulse® 1370 ABS + Polycarbonate
PULSE® 1370 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM Data
Styron Pulse® 600 ABS + Polycarbonate
PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM Data
Styron Pulse® 710 ABS + Polycarbonate
PULSE® 710 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 710 Engineering resin h..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM Data
Styron Pulse® 830 ABS + Polycarbonate
PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D412
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Ecomass® 1050ZB92 Filled Polyamide
Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyGood ToughnessInformation provided by Technical Polymers
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Ecomass® 1700TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Po..
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Ecomass® 1850ZG90 Metal Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D638
Ecomass® 1850ZG92 Metal Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityMetal Powder Filled Polyamide (PA6)Information provided by Technical Polymers
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM D412
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Tensile Strength, Ultimate 44.8 - 160 MPa
6500 - 23200 psi
Average value: 87.1 MPa Grade Count:21
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..