Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Pacific Sintered Materials FN-253-S(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Kennametal Stellite Deloro® 208 PM after P/M Processing Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s.. |
|||
Tensile Strength, Ultimate | 690 MPa @Temperature 649 °C |
100000 psi @Temperature 1200 °F |
|
Kennametal Stellite Stellite® 3 PM with P/M Processing Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
Tensile Strength, Ultimate | 689 - 724 MPa | 100000 - 105000 psi | |
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
MetalTek MTEK 420 Cast UNS J91153 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
MetalTek MTEK 6 UNS R30006 Cobalt Base Alloy Non-galling, heat and thermal shock resistance. Heat Resistance.Applications: Bearings and hot work sleeves, housings. Rocket engine partsInformation provided by MetalTek |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Haynes Hastelloy® G-30® alloy, mill annealed HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Ultimate | 690 - 920 MPa @Diameter 6.35 mm |
100000 - 133000 psi @Diameter 0.250 in |
CWSR; DAN 2700.9 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Ultimate | 690 MPa @Temperature 538 °C |
100000 psi @Temperature 1000 °F |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | (Tensile Yield Strength near U.T.S.) |
Kennametal Stellite Stellite® 12 Satisfactory finishing results can be obtained using carbide tipped tools. Applications include cutting plastics, rubber, paper, carpet, and wood; saw teeth, trimmer knives, carpet knives, ledger bl.. |
|||
Tensile Strength, Ultimate | 689 - 1170 MPa | 100000 - 170000 psi | |
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe.. |
|||
Tensile Strength, Ultimate | 689 - 827 MPa | 100000 - 120000 psi | |
Meehanite HSV Heat Resisting Cast Iron Type HSV is an iron developed essentially for engineering parts subjected to long continuous heating. It has been designed to have the maximum load bearing ability.General Meehanite information - M.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | Annealed |
Special Metals INCOLOY® Alloy 825 A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | Heat Treated |
Universal Wire Works 29-9 (AMS 5784) Filler Metal Universal 29-9 is designed for welding similar and dissimilar corrosion and heat resisting steels with the gas metal arc and gas tungsten arc welding processes.Information provided by Universal Wire.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
Universal Wire Works C-276 Nickel Alloy Welding Wire Alloy C-276 is a low carbon, nickel base alloy containing significant amounts of molybdenum and chromium. Alloy C-276 is one of the most universally corrosion resistant alloys available. This alloy .. |
|||
Tensile Strength, Ultimate | 689 - 786 MPa | 100000 - 114000 psi | |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | |
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 405 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 689 MPa | 100000 psi | cold worked |
CMW® ELKONIUM 42 palladium based alloy Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 692 MPa @Temperature 93.3 °C |
100000 psi @Temperature 200 °F |
Sheet |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allegheny Ludlum Grade 4 Titanium (UNS R50700) Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Ultimate | 690 - 800 MPa | 100000 - 116000 psi | |
ArcelorMittal TRIP 690 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT690T), electrogalvanized (HCT690T+ZE) and Extragal®/Galvannealed (HCT690T+Z)Description: TRIP steels offer an outstanding combination of strength and ductil.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal Data provided by Allvac.Applications: Afterburner components, combustion chamber liners, nozzles, vanes, rings, turbine exhaust weldments, structural parts. |
|||
Tensile Strength, Ultimate | >= 690 MPa | >= 100000 psi | |
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276 AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | |
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Tensile Strength, Ultimate | 690 MPa | 100000 psi | typical |
ATI Allegheny Ludlum AL 825™ Nickel Alloy Allegheny Ludlum AL 825 alloy is an austenitic nickel-iron-chromium-molybdenum-copper alloy containing high levels of corrosion resistance to both moderately oxidizing and moderately reducing enviro.. |