Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encountered in the chemical and petrochemical processing, flue gas desulfurization, pulp and paper and other specialized fields. Design of the alloy allows a high level of corrosion resistance to be retained even in the welded condition.This alloy also has good high temperature strength and moderate oxidation resistance although the alloy will eventually form embrittling high temperature precipitates. It has been available for several years and has been used in ASME Boiler and Pressure Vessel related construction. The alloy is readily fabricated by welding using techniques similar to those used for austenitic stainless steels and other nickel base alloys. Precautions are advisable during fabrication because raising the low carbon and silicon contents of the material may adversely affect important properties.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 8.90 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B <= 100
<= 100
Tensile Strength, Ultimate >= 690 MPa
>= 100000 psi
Tensile Strength, Yield >= 283 MPa

@Strain 0.200 %
>= 41000 psi

@Strain 0.200 %
Elongation at Break >= 40 %
>= 40 %
in 2"
Modulus of Elasticity 205 GPa
29700 ksi
Charpy Impact 325 J
240 ft-lb
10 mm sample from annealed plate
Thermal Properties Metric English Comments
CTE, linear 11.2 µm/m-°C

@Temperature 20.0 - 93.0 °C
6.22 µin/in-°F

@Temperature 68.0 - 199 °F
12.8 µm/m-°C

@Temperature 20.0 - 315 °C
7.11 µin/in-°F

@Temperature 68.0 - 599 °F
13.4 µm/m-°C

@Temperature 20.0 - 538 °C
7.44 µin/in-°F

@Temperature 68.0 - 1000 °F
Specific Heat Capacity 0.425 J/g-°C
0.102 BTU/lb-°F
Thermal Conductivity 10.2 W/m-K
70.8 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.0040 %
0.0040 %
Chromium, Cr 15.5 %
15.5 %
Cobalt, Co 0.10 %
0.10 %
Iron, Fe 6.0 %
6.0 %
Manganese, Mn 0.15 %
0.15 %
Molybdenum, Mo 16 %
16 %
Nickel, Ni 59 %
59 %
as balance
Phosphorous, P 0.0050 %
0.0050 %
Silicon, Si 0.030 %
0.030 %
Sulfur, S 0.0020 %
0.0020 %
Tungsten, W 3.5 %
3.5 %
Vanadium, V 0.15 %
0.15 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000130 ohm-cm
0.000130 ohm-cm
Magnetic Permeability 1.02
1.02