ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Allvac.Applications: Afterburner components, combustion chamber liners, nozzles, vanes, rings, turbine exhaust weldments, structural parts.
Physical Properties Metric English Comments
Density 8.22 g/cc
0.297 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Tensile Strength, Ultimate 690 MPa
100000 psi
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Elongation at Break 40 %
40 %
Reduction of Area 45 %
45 %
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 21.75 %
21.75 %
Cobalt, Co 1.5 %
1.5 %
Iron, Fe 18.5 %
18.5 %
Molybdenum, Mo 9.0 %
9.0 %
Nickel, Ni 49 %
49 %
Tungsten, W 0.60 %
0.60 %