Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.0 - 85.0 MPa @Temperature 60.0 - 150 °C |
1740 - 12300 psi @Temperature 140 - 302 °F |
Average value: 41.5 MPa Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Ultimate | 25.0 - 85.0 MPa @Temperature 60.0 - 120 °C |
3630 - 12300 psi @Temperature 140 - 248 °F |
Average value: 60.0 MPa Grade Count:2 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 38.0 - 85.0 MPa @Temperature 60.0 - 120 °C |
5510 - 12300 psi @Temperature 140 - 248 °F |
Average value: 58.4 MPa Grade Count:3 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Tensile Strength, Ultimate | 19.3 - 85.0 MPa | 2800 - 12300 psi | Average value: 64.0 MPa Grade Count:200 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 13.8 - 85.0 MPa | 2000 - 12300 psi | Average value: 62.3 MPa Grade Count:11 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Tensile Strength, Ultimate | 40.0 - 85.0 MPa @Temperature 60.0 - 90.0 °C |
5800 - 12300 psi @Temperature 140 - 194 °F |
Average value: 78.1 MPa Grade Count:12 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |