Tensile Strength, Ultimate |
51.0 - 69.0 MPa |
7400 - 10000 psi |
Average value: 58.0 MPa Grade Count:10 |
Overview of materials for Phenolic, Resole, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |
Tensile Strength, Ultimate |
41.0 - 69.0 MPa |
5950 - 10000 psi |
|
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer. |