Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -45.0 °C |
23.8 ft-lb/in² @Temperature -49.0 °F |
ISO 180/1eA |
Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled Heat stabilized, black colorInformation provided by PolyPlastic Group. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Thickness 4.00 mm, Temperature -20.0 °C |
23.8 ft-lb/in² @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PE 1295 PRE-ELEC PE 1295 is a dissipative thermoplastic compound based on PE-HD. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resistance bet.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U |
Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 BR20 NL100 HS PBT, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GB30 NL PA6, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -25.0 °C |
23.8 ft-lb/in² @Temperature -13.0 °F |
ISO 179/1eU |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 25.0 °C |
23.8 ft-lb/in² @Temperature 77.0 °F |
ISO 179/1eU |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Izod Impact, Unnotched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |