Mechanical Properties Metric English Comments
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 500 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 500 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 1000 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 500 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 1000 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-135N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PT-170 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PTA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 110 °C,
Time 86400 sec
711 - 1420 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 1350 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 4.90 - 9.81 MPa

@Temperature 1500 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).