Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories PAC-160 Plastic Refractory

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories PAC-160 Plastic Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 3.37e-7 - 0.000491 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000489 - 0.0711 ksi

@Temperature 230 °F,
Time 24.0 hour
0.000981 - 0.003924 GPa

@Temperature 1350 °C,
Time 10800 sec
0.142 - 0.5691 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.000981 - 0.003924 GPa

@Temperature 1500 °C,
Time 10800 sec
0.142 - 0.5691 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
4.90 - 9.81 MPa

@Temperature 1350 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
4.90 - 9.81 MPa

@Temperature 1500 °C,
Time 10800 sec
711 - 1420 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.9305 W/m-K

@Temperature 500 °C
6.447 BTU-in/hr-ft²-°F

@Temperature 932 °F
1.0236 W/m-K

@Temperature 1000 °C
7.0921 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
limited
Shrinkage -1.50 %

@Temperature 110 °C,
Time 86400 sec
-1.50 %

@Temperature 230 °F,
Time 24.0 hour
0.20 %

@Temperature 1500 °C,
Time 10800 sec
0.20 %

@Temperature 2730 °F,
Time 3.00 hour
0.65 %

@Temperature 1350 °C,
Time 10800 sec
0.65 %

@Temperature 2460 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
SiC 17 - 23 %
17 - 23 %
Descriptive Properties Value Comments
Main Applications Corrosion resistant Cupola Spout
Material Required for Estimating (kg/?) 2,260